Ground Coat Enamel Frits
Date:2021-12-03 Categories:related product
Post Date: |
Dec 02,2021 |
Expiry Date: |
Dec 02,2022 |
Detailed Description: |
Ground Coat and One-coat Enamel Frits Reference No. Description Expansion Firing Coefficient (10-7) Temperature (° C) UNG-102 High Temp.Nickel Ground Coat 301.8 840-880 UNG-103 High Temp.Nickel Ground Coat 286.5 860-890 UNG-104 High Temp.Nickel Ground Coat 290.1 840-880 UNG-105 High Temp. Antimony Molybdenum White Ground Coat 297.1 840-870 UNG-111 Medium Temp.Co-Ni Ground Coat 313.7 800-840 UNG-112 Medium Temp.Co-Ni Ground Coat 292.1 820-860 UNG-118 Medium Temp.Nickel Ground Coat 309.1 800-840 UNG-124 Low Temp. Antimony Molybdenum White Ground Coat 290.1 780-820 UNG-1102 High Temp.Co-Ni Ground Coat 300.5 840-880 UNG-1112 Medium Temp.Co-Ni Ground Coat 283.6 830-860 UNG-1122 Low temp.Co-Ni Ground coat 300.5 780-820 UNG-2400 Low Temp.Co-Ni Ground Coat 322.1 760-800 UNG-2401 Medium temp.Co-Ni Ground Coat 292.1 800-840 UNG-2404 High Temp.Co-Ni Ground Coat 290.1 840-870 UNG-2405 High Yemp.Co-Ni Ground Coat 288.1 860-880 UNG-2406 Temp. Resistant Co-Ni Ground Coat 278.2 860-900 UNG-2414 Low Temp. Co-Ni Ground Coat 311.1 760-800 UNG-2115 One-coat Black Enamel 296.1 830-850 Remarks: directly coated on base metal.with strong adherence. wide range of firing temperature. 1. Mill Addition Ratio for Nickel and Co-Ni Ground Coat: Frit 100 Clay 5-7 Quartz porwder 0-8 Borax 0.3- 0.5 Sodium Nitrite 0.2-0.3 Water 50- 55ml 2. Mill Addition Ratio of Sb-Mo Ground Coat: Frit 100 Antimony Oxide 1.0 Clay 5-7 Barium Molybdate 1.0 Quartz Powder 0-8 Water 50-55 ml Frit Slurry Fineness 1- 2g/150mesh.100ml Specific Gravity 160-170g/100 ml |